Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00270 GPa
0.392 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBT
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00270 GPa
0.392 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 4.0 PHR MBTS
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00270 GPa
0.392 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re..
100% Modulus 0.00270 GPa
0.392 ksi
Die C; Cross direction; ASTM D412
Teknor Apex Sarlink® 4465 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4465 is a low hardness grade possessing exceptional tensile strength, superior compression s..
100% Modulus 0.00270 GPa
0.392 ksi
DuPont Vamac® GXF Sample Compound Vulcanizate Slab Cure (5 minutes at 190°C)
Test slab is cured for 5 minutes at 190°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for their own ..
100% Modulus 0.00270 GPa
0.392 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Zinc Stearate
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00270 GPa
0.392 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 4.0 PHR MBTS
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00270 GPa
0.392 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR MBT
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00270 GPa
0.392 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® STK55PA Thermoplastic Elastomer
Elastocon® STK55PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK55PA is well suited for consumer go..
100% Modulus 0.00270 GPa
0.392 ksi
ISO 37
AlphaGary Evoprene™ COGEE 683 SEBS Thermoplastic Elastomer
Evoprene™ COGEE was developed to comold or coextrude with engineered thermoplastics and designed for soft touch applications.Processing: compatible with polypropylene and polystyrene for co-molding..
100% Modulus 0.00270 GPa
0.392 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Zinc Stearate
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
100% Modulus 0.00270 GPa
0.392 ksi
ISO 37
AlphaGary Evoprene™ GC 5650 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..