Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 0.950 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
23/23°C; ASTM D792
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 0.950 - 1.45 g/cc
0.950 - 1.45 g/cc
ASTM D792
Parker Chomerics Tecknit SC-Consil® 864 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
ExxonMobil Vyram™ 9203-45 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
Specific Gravity 0.950 g/cc
0.950 g/cc
ISO 1183
GEHR Plastics PE-HD Polyethylene HDPE
Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature is from -50..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Teknor Apex Telcar® OBC 1383N Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Specific Gravity 0.950 g/cc
0.950 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 391E Ionomer
Information provided by A. Schulman.
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYBATCH™ 10178 Amber Concentrate Based in LDPE
DescriptionPOLYBATCH® Amber 10178 is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178 is designed for use between 3 and 5% HDPE molded bottles (approx. 50 mil) to achieve 90%..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
DuPont Surlyn® 8945 Thermoplastic Ionomer Resin
Surlyn® 8945 provides high flow properties and consistent, easy processing in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the ionomer sp..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D1505
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer
DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYBATCH™ 10178 Amber Concentrate Based in LDPE
DescriptionPOLYBATCH® Amber 10178 is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178 is designed for use between 3 and 5% HDPE molded bottles (approx. 50 mil) to achieve 90%..
Specific Gravity 0.950 g/cc
0.950 g/cc
Zeon Chemicals Nipol® 1014 Nitrile Elastomer
Nipol 1014 is a copolymer of butadiene and acrylonitrile with low oil resistance designed to provide a maximum of low temperature flexibility. Sufficient antioxidant is added during manufacture for ..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYBATCH™ 10178 Amber Concentrate Based in LDPE
DescriptionPOLYBATCH® Amber 10178 is an amber color concentrate based in LDPE. ApplicationPOLYBATCH® 10178 is designed for use between 3 and 5% HDPE molded bottles (approx. 50 mil) to achieve 90%..
Specific Gravity 0.950 g/cc
0.950 g/cc
Zeon Chemicals Zetpol® 2020L Hydrogenated Nitrile Elastomomer
Zetpol 2020L is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance ..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 2388 Glass Reinforced Polypropylene
DescriptionPolyfort® FPP 2388 is a 5% glass reinforced polypropylene.Information provided by A. Schulman.
Specific Gravity 0.950 g/cc
0.950 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 391E Ionomer
Information provided by A. Schulman.
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass)
DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYBATCH™ XAMF-500-T Process Aid Concentrate, Concentrate Based In LLDPE
DescriptionPOLYBATCH® XAMF-500-T is a 5% active, multicomponent, process aid concentrate based in LLDPE. This concentrate is designed for use in unfilled systems to reduce/eliminate melt fracture...
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYBATCH™ Blue 40460/4 Concentrate Based In LLDPE
DescriptionPOLYBATCH® 40460/4 is a blue color concentrate based in LLDPE. This concentrate was designed to provide color in blow molding applications. POLYBATCH® 40460/4 is typically recommended..
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
E-Polymers EFLEX® I2020 Ionomer
I-series (Ionomer): E-FLEX Ionomer is a family of ethylene acrylic acid (E/AA) copolymers, in which part of the acrylic acid is neutralized with metal ions such as zinc (Zn) or sodium (Na) or magnes..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
E-Polymers EFLEX® I2030 Ionomer
I-series (Ionomer): E-FLEX Ionomer is a family of ethylene acrylic acid (E/AA) copolymers, in which part of the acrylic acid is neutralized with metal ions such as zinc (Zn) or sodium (Na) or magnes..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
Asia Technology Pioneers CAP 502 PP Nanocomposite
Description: CAP502 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
PolyOne Synprene® IT 705 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedOpaqueApplications:Multi-PurposeGaskets and SealsProcessing Method:ExtrusionPolyOne First ChoiceInformation provided by Poly..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
PolyOne Synprene® RT-3945 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
PolyOne Synprene® RT-3955 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti..
Specific Gravity 0.950 g/cc
0.950 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance ..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene
DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati..
Specific Gravity 0.950 g/cc
0.950 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 2388 Glass Reinforced Polypropylene
DescriptionPolyfort® FPP 2388 is a 5% glass reinforced polypropylene.Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved