Polymer Property : 100% Modulus = 0.00117 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00117 GPa
0.170 ksi
ASTM D412
Huntsman IROGRAN® PS 455-204 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
100% Modulus 0.00117 GPa
0.170 ksi
ASTM D3574E
Mearthane Durethaneâ„¢ M DM-640A Foam Polyurethane
MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur..
100% Modulus 0.00117 GPa
0.170 ksi
ASTM D412
Teknor Apex UNIPRENE® 7010-45 Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00117 GPa
0.170 ksi
ASTM D 412
CPT C-Flex® R70-050 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
100% Modulus 0.00117 GPa
0.170 ksi
ASTM D412
Advanced Polymer Alloys DuraGrip™ 6140 NC Thermoplastic Elastomer
DuraGrip® 6140NC is an enhanced bonding and adhesion grade Thermoplastic Elastomer (TPE) designed for injection molding and extrusion processes. It will bond well with polycarbonate, polycarbonate ..
100% Modulus 0.00117 GPa
0.170 ksi
ASTM D412
3M SJ-1FB Cold Shrink Foldback Splice Jacket Kits
3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice..
100% Modulus 0.00117 GPa
0.170 ksi
ASTM D412
3M SJ-2FB Cold Shrink Foldback Splice Jacket Kits
3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice..
100% Modulus 0.00117 GPa
0.170 ksi
ASTM D412
3M SJ-3FB Cold Shrink Foldback Splice Jacket Kits
3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice..
100% Modulus 0.00117 GPa
0.170 ksi
ASTM D412
3M SJ-4FB Cold Shrink Foldback Splice Jacket Kits
3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice..