Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 60.7 MPa | 8800 psi | ASTM D638 |
Nylene® Naxel™ PC30 Polycarbonate Description: Naxel™ PC30 is a 25 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources .. |
|||
Tensile Strength, Ultimate | 60.7 MPa | 8800 psi | ASTM D638 |
Nylene® Naxel™ PC502 10% Glass Reinforced Polycarbonate Description: Naxel™ PC502 is a 10% glass fiber reinforced polycarbonate. PC502 is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companie.. |
|||
Tensile Strength, Ultimate | 60.7 MPa | 8800 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PS-25MN/000 Polybutylene Terephthalate (PBT), Mineral Filled
(discontinued **) Description/Features:Mineral FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 60.7 MPa | 8800 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-03CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 60.7 MPa | 8800 psi | ASTM D638 |
Adell AI-10 Nylon 66, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 60.7 MPa | 8800 psi | |
Abatron AboCast 7703-21/AboCure 7703-21 (A) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Tensile Strength, Ultimate | 60.7 MPa | 8800 psi | ASTM D638 |
Nylene® Naxel™ PC40CV Polycarbonate Description: Naxel™ PC40CV is a 17 melt, virgin, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric .. |
|||
Tensile Strength, Ultimate | 60.7 MPa | 8800 psi | ASTM D638 |
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 60.7 MPa | 8800 psi | 0.2 in/min;ASTM D638 |
Styrolution NAS® 30 Series High Performance Styrenic It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class.. |
|||
Tensile Strength, Ultimate | 60.7 MPa | 8800 psi | ASTM D638 |
Adell AI-30 Nylon 66, Impact Modified Data provided by Adell Plastics, Inc. |