Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.30 GPa | 479 ksi | |
Plastcom SLOVAMID 6/66 FRc 3 TS PA6/66, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 + PA 66 alloy for injection moulding with increased flammability resistance, with nonhalogen flame retardant. Excellent.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 1% Secant at 0.05 in/min; ASTM D790 |
North Wood Plastics Polypropylene with 40% Wood Fiber, Molding Grade Data provided by North Wood Plastics, Inc. |
|||
Flexural Modulus | 3.30 - 16.7 GPa @Thickness 0.800 - 3.17 mm |
479 - 2420 ksi @Thickness 0.0315 - 0.125 in |
Average value: 7.38 GPa Grade Count:2 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Flexural Modulus | 3.30 - 7.60 GPa | 479 - 1100 ksi | Average value: 4.83 GPa Grade Count:4 |
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D790 |
Lucky EG-920 Acrylic, Extrusion Grade Special extrusion grade with excellent stress cracking resistance, intended mainly for exterior applications. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, hi.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D790 |
Lucky EG-930 Acrylic, Injection Grade Injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D790 |
Lucky IG-840 Acrylic, Injection Grade General purpose injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and col.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ISO 178 |
LyondellBasell Astryn EPKT25M Polypropylene Copolymer, Mineral Filled Key Features: conventional melt flow, very high modulus, mineral-filled polypropylene copolymer, high rigidity, good impact resistance, good dimensional stability, low foggingApplications: glove box.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1000FV PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1000R PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1010F PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1010K PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1010V PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). UL94 V0, V2 and 5VA listing. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem MD130A PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant, ISO 10993 compliant in recognized colors.This data was supplied by SABIC-IP for the Europe-.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp PH0600B PA 6 LNP* Thermocomp* PH0600B is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1000EF PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RB004 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RB004 is a compound based on PA 66 resin containing Glass Beads.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM-D790 |
Polyram PlusTek PA340S6 Nylon 6.6, 30% Glass beads 30% glass beads reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ISO 178-93 |
Wellman Wellamid® MRT1487 BK 32% Mineral Reinforced, Toughened Grade Nylon 66 Description: Mineral Reinforced, Toughened Grade Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
Eurostar Starflam AFR200Y PA66, Flame Retardant, Injection Molding Staramide AFR200Y is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD4471 PC (Asia Pacific) Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D790 |
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |