Polymer Property : Tensile Strength, Ultimate = 8800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 60.7 MPa
8800 psi
ASTM D638
Nylene® Naxel™ PC30 Polycarbonate
Description: Naxel™ PC30 is a 25 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources ..
Tensile Strength, Ultimate 60.7 MPa
8800 psi
ASTM D638
Nylene® Naxel™ PC502 10% Glass Reinforced Polycarbonate
Description: Naxel™ PC502 is a 10% glass fiber reinforced polycarbonate. PC502 is UL approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companie..
Tensile Strength, Ultimate 60.7 MPa
8800 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® PS-25MN/000 Polybutylene Terephthalate (PBT), Mineral Filled  (discontinued **)
Description/Features:Mineral FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 60.7 MPa
8800 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® AS-03CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 60.7 MPa
8800 psi
ASTM D638
Adell AI-10 Nylon 66, Impact Modified
Data provided by Adell Plastics, Inc.
Tensile Strength, Ultimate 60.7 MPa
8800 psi
Abatron AboCast 7703-21/AboCure 7703-21 (A) Epoxy Adhesive and Casting Compound
AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane..
Tensile Strength, Ultimate 60.7 MPa
8800 psi
ASTM D638
Nylene® Naxel™ PC40CV Polycarbonate
Description: Naxel™ PC40CV is a 17 melt, virgin, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric ..
Tensile Strength, Ultimate 60.7 MPa
8800 psi
ASTM D638
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
Tensile Strength, Ultimate 60.7 MPa
8800 psi
0.2 in/min;ASTM D638
Styrolution NAS® 30 Series High Performance Styrenic
It has sparkling clarity and good scratch resistance. This easily processed copolymer blends well with K-Resin® to modify flexibility, surface hardness, and HDT. It meets USP XXIII Spec. of Class..
Tensile Strength, Ultimate 60.7 MPa
8800 psi
ASTM D638
Adell AI-30 Nylon 66, Impact Modified
Data provided by Adell Plastics, Inc.