Addiplast Addinyl PMD 20090 Nylon 6, 40% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer Addiplast
Trade Name Addinyl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addinyl PMD 20090 Nylon 6, 40% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber reinforced, high resistance to frictionInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
Conditioned; ISO 868
84
84
ISO 868
Tensile Strength at Break 90.0 MPa
13100 psi
Conditioned; ISO R 527
130 MPa
18900 psi
ISO R 527
Elongation at Yield 5.0 %
5.0 %
ISO R 527
8.0 %
8.0 %
Conditioned; ISO R 527
Modulus of Elasticity 4.75 GPa
689 ksi
Conditioned; ISO 178
8.30 GPa
1200 ksi
ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
ISO 180/1A
32.0 kJ/m²
15.2 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
ISO 179/IeU
4.50 J/cm²
21.4 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/IeA
2.50 J/cm²
11.9 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
ASTM E831
Melting Point 220 °C
428 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-2/AF
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
CEI 60112/Solution A
Users viewing this material also viewed the following: