Material Notes:
Flame retardant, halogen freeInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 77
77
Conditioned; ISO 868
83
83
ISO 868
Tensile Strength at Break 45.0 MPa
6530 psi
Conditioned; ISO R 527
60.0 MPa
8700 psi
ISO R 527
Tensile Strength, Yield 40.0 MPa
5800 psi
Conditioned; ISO R 527
75.0 MPa
10900 psi
ISO R 527
Elongation at Break 10 %
10 %
ISO R 527
30 %
30 %
Conditioned; ISO R 527
Modulus of Elasticity 1.00 GPa
145 ksi
Conditioned; ISO 178
3.00 GPa
435 ksi
ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180/1A
10.0 kJ/m²
4.76 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched NB
NB
ISO 179/IeU
NB
NB
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179/IeA
1.00 J/cm²
4.76 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75-2/AF
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Oxygen Index 30 %
30 %
ISO 4589
Glow Wire Test 960 °C
1760 °F
CEI 60695/2/1
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Conditioned; CEI 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
Conditioned; CEI 60093
1.00e+14 ohm
1.00e+14 ohm
CEI 60093
Dielectric Strength 26.0 kV/mm
660 kV/in
CEI 60243-1
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A