Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adamas Adalon® 808 PTFE, Bronze + PEEK+ Carbon Fiber

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Bronze Filled , Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
Manufacturer Adamas
Trade Name Adalon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adamas Adalon® 808 PTFE, Bronze + PEEK+ Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 2.28 - 2.32 g/cc
2.28 - 2.32 g/cc
ASTM D792
Deformation 1.7 - 3.0 %
1.7 - 3.0 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 58 - 60
58 - 60
ASTM D2240
Ball Indentation Hardness 54.0 - 56.0 MPa
7830 - 8120 psi
ISO 2032
Tensile Strength at Break 3.00 - 4.00 MPa
435 - 580 psi
ASTM D4745-97
Elongation at Break 3.0 - 5.0 %
3.0 - 5.0 %
ASTM D4745-97
Coefficient of Friction, Static 0.10 - 0.30
0.10 - 0.30
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.820 W/m-K
5.69 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 270 °C
518 °F
DSC
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
ASTM D257
Surface Resistance 1.00e+6 ohm
1.00e+6 ohm
ASTM D257