Polymer Property : Ball Indentation Hardness = 8120 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 38.0 - 56.0 MPa
5510 - 8120 psi
Average value: 50.3 MPa Grade Count:4
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum ..
Ball Indentation Hardness 52.0 - 56.0 MPa
7540 - 8120 psi
ISO 2032-N961
Adamas Adalon® 113 PTFE, 23/2% Carbon/Graphite Filled
Information provided by Adamas, HPM
Ball Indentation Hardness 54.0 - 56.0 MPa
7830 - 8120 psi
ISO 2032
Adamas Adalon® 808 PTFE, Bronze + PEEK+ Carbon Fiber
Information provided by Adamas, HPM
Ball Indentation Hardness 54.0 - 56.0 MPa
7830 - 8120 psi
ISO 2032
Adamas Adalon® 477 PTFE, 20% Aramid Fiber
Information provided by Adamas, HPM
Ball Indentation Hardness 52.0 - 56.0 MPa
7540 - 8120 psi
ISO 2032-N961
Adamas Adalon® 131 PTFE, 25% Soft Carbon Filled
Information provided by Adamas, HPM