Thermal Properties Metric English Comments
Thermal Conductivity 0.820 W/m-K
5.69 BTU-in/hr-ft²-°F
Schott N-LASF44 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.820 W/m-K
5.69 BTU-in/hr-ft²-°F
Schott N-LAK34 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.820 W/m-K
5.69 BTU-in/hr-ft²-°F
ASTM C 177
Adamas Adalon® 509 PTFE, 3% MoS2
Information provided by Adamas, HPM
Thermal Conductivity 0.820 W/m-K
5.69 BTU-in/hr-ft²-°F
ASTM C 177
Adamas Adalon® 808 PTFE, Bronze + PEEK+ Carbon Fiber
Information provided by Adamas, HPM
Thermal Conductivity 0.820 W/m-K
5.69 BTU-in/hr-ft²-°F
ASTM C 177
Adamas Adalon® 508 PTFE, 1% MoS2
Information provided by Adamas, HPM
Thermal Conductivity 0.820 W/m-K
5.69 BTU-in/hr-ft²-°F
ASTM C 177
Adamas Adalon® 510 PTFE, 5% MoS2
Information provided by Adamas, HPM
Thermal Conductivity 0.820 W/m-K
5.69 BTU-in/hr-ft²-°F
ASTM C 177
Adamas Adalon® 600 PTFE, Boro Nitruro
Information provided by Adamas, HPM