Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Copolymer CP0437M40L Mica Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Mica Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0437M40L Mica Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
MD; ASTM D955
Melt Flow 15 g/10 min
15 g/10 min
ASTM D1238
Ash 40 %
40 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 33
33
ASTM D785
Tensile Strength at Break 14.0 MPa
2030 psi
ASTM D638
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Tensile Modulus 2.499 GPa
362.5 ksi
ASTM D638
Flexural Strength 22.0 MPa
3190 psi
ASTM D790
Flexural Modulus 3.000 GPa
435.1 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C
145 °F