Polymer Property : Tensile Modulus = 2.499 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.499 GPa
362.5 ksi
ASTM D638
Aclo Accutech ABS ABS834G10L Glass Reinforced
Tensile Modulus 2.499 GPa
362.5 ksi
ASTM D638
Aclo Accutech Polyethylene HD0232G20CV High Density Glass Reinforced Chemically Coupled
Approved to GMP.PE.018 Black A12438
Tensile Modulus 2.499 GPa
362.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437G20CL Glass Reinforced Coupled
Tensile Modulus 2.499 GPa
362.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0437M40L Mica Reinforced
Tensile Modulus 2.499 GPa
362.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0336T40L Talc Reinforced
Tensile Modulus 2.499 GPa
362.5 ksi
ASTM D638
Aclo Accutech Polypropylene Copolymer CP0436G20CL Glass Reinforced
Tensile Modulus 2.499 GPa
362.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339M20CL Mica Reinforced Coupled
Tensile Modulus 2.499 GPa
362.5 ksi
ASTM D638
Aclo Accutech Polypropylene Homopolymer HP0339M20L Mica Reinforced