Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 8005-6/AboCure 8005-6 Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8005-6/AboCure 8005-6 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboCast 8005-6 is a tan, viscous filled liquid resin with a weight of approximately 11 lbs/gallon. AboCure 8005-6 is an amber, viscous liquid converter with a weight of approximately 10 lbs/gallon. AboCast 8005-6/AboCure 8005-6 is a 2-component clear epoxy system for industrial, architectural, and marine uses. It bonds new concrete to old with a stronger-than-concrete bond between wet-poured concrete and old concrete. It makes it possible to resurface concrete with thin, light-weight layers of concrete and terrazzo. It is used as a bonding agent for restoring bridges, runways, ramps, decks, driveways, and commercial and residential buildings, avoiding costly replacement. AboCast 8005-6/AboCure 8005-6 is easy to apply with a brush or roller. It is outstanding for resurfacing floors and can be extended with fillers like sand, gravel, or chips. It is excellent for functional and decorative non-skid floors. It is also chemically resistant and easy to color. 100% epoxy solids. 7/3 ratio by volume. 30-40 minute working life. Hardens in 0.5-3 hours on wet or cold surfaces.
Processing Properties Metric English Comments
Cure Time 30.0 - 60.0 min

@Temperature 80.0 - 120 °C
0.500 - 1.00 hour

@Temperature 176 - 248 °F
2880 - 10080 min

@Temperature 20.0 °C
48.0 - 168.0 hour

@Temperature 68.0 °F
(2-7 Days)
Pot Life 30 - 40 min

@Temperature 25.0 °C
30 - 40 min

@Temperature 77.0 °F
100 g
Descriptive Properties Value Comments
Hardening Time (min) 30-180