Processing Properties Metric English Comments
Cure Time 2880 - 10080 min

@Temperature 20.0 °C
48.0 - 168.0 hour

@Temperature 68.0 °F
(2-7 Days)
Abatron AboCast 8005-6/AboCure 8005-6 Epoxy
AboCast 8005-6 is a tan, viscous filled liquid resin with a weight of approximately 11 lbs/gallon. AboCure 8005-6 is an amber, viscous liquid converter with a weight of approximately 10 lbs/gallon. ..
Cure Time 7200 - 10080 min

@Temperature 15.556 - 26.667 °C
120 - 168.0 hour

@Temperature 60.001 - 80.001 °F
(5-7 Days)
Abatron AboTar 8101-8 Solventless Tar-Epoxy Compound
AboTar 8101-8 is a 2-part tar-epoxy variable-ratio system. It is weather- and water-proof, flexible, and acid, alkali, and fuel resistant. It can be used neat or with sand or aggregates. Uses: Resu..
Cure Time 7200 - 10080 min

@Temperature 24.0 °C
120 - 168.0 hour

@Temperature 75.2 °F
full cure
BCC Products BC 8782 Urethane Casting
BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readi..
Cure Time 7200 - 10080 min

@Temperature 24.0 °C
120 - 168.0 hour

@Temperature 75.2 °F
complete cure
BCC Products BC 8880 Polyurethane Elastomer Surface Coat
BC8880 is a two-part urethane gel coat which exhibits excellent handling characteristics and very low moisture sensitivity. Its characteristics include a high modulus and a high hardness. It is a br..