Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROLENE® ARPS 100-1 GPPS BLACK Polystyrene Compounded Resin

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer Aaron Industries Corporation
Trade Name AAROLENE® ARPS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROLENE® ARPS 100-1 GPPS BLACK Polystyrene Compounded Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A reprocessed, general-purpose Polystyrene resin, compounded black, specifically designed for all high speed injection molding applications.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 12 g/10 min

@Load 5.00 kg,
Temperature 200 °C
12 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.3 MPa
5700 psi
ASTM D638
Flexural Modulus 3.03 GPa
440 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
ASTM D648