ATI Allegheny Ludlum AL 36™ Electrical Alloy (Cryogenic and Bimetal) UNS K93600 or UNS K93603

Category Metal , Electronic/Magnetic Alloy , Ferrous Metal
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AL 36™ Electrical Alloy (Cryogenic and Bimetal) UNS K93600 or UNS K93603.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AL 36 alloy is a nickel-iron alloy combining low thermal expansion properties up to about 200°C along with moderately high strength and good toughness down to -235°C, the temperature of liquid hydrogen. These properties combined with good weldability and desirable physical properties make this alloy attractive for many applications requiring precise dimensional stability. In applications such as LNG tankers and in transportation and storage vessels for liquefied gas, AL 36 alloy is at an advantage due to the minimization of any strains in the material resulting from thermal contraction. The composition of AL 36 alloy for cryogenic application is adjusted to achieve very low thermal expansion coefficient at low temperature. This alloy is also used extensively in the manufacture of bimetallic components for electrical and electronic industries. It is the low expansion material used in the cladding o high expansion alloys, such as AL 22-3.Information provided by Allegheny Ludlum
Physical Properties Metric English Comments
Density 8.05 g/cc
0.291 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 75
75
Typical Annealed
Tensile Strength, Ultimate 462 MPa
67000 psi
Typical Annealed
Tensile Strength, Yield 261 MPa

@Strain 0.200 %
37900 psi

@Strain 0.200 %
Typical; Annealed
Elongation at Break 32 %
32 %
typical in 2"; Annealed
Thermal Properties Metric English Comments
CTE, linear 0.500 - 1.10 µm/m-°C

@Temperature 25.0 - 93.0 °C
0.278 - 0.611 µin/in-°F

@Temperature 77.0 - 199 °F
2.00 - 2.70 µm/m-°C

@Temperature 25.0 - 260 °C
1.11 - 1.50 µin/in-°F

@Temperature 77.0 - 500 °F
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.030 %
<= 0.030 %
Carbon, C 0.0080 %
0.0080 %
Cobalt, Co <= 0.35 %
<= 0.35 %
Iron, Fe 63 %
63 %
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo <= 0.020 %
<= 0.020 %
Nickel, Ni 36 %
36 %
Silicon, Si 0.15 %
0.15 %
Sulfur, S 0.0010 %
0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000810 ohm-cm
0.0000810 ohm-cm