Plenco 51030 PET, Pellet, Injection Molded, Natural Color  (discontinued **)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 51030 PET, Pellet, Injection Molded, Natural Color  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 51030 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage 0.00070 cm/cm
0.00070 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 164.7 MPa
23890 psi
ASTM D638
Elongation at Break 2.17 %
2.17 %
ASTM D638
Tensile Modulus 11.27 GPa
1635 ksi
ASTM D638
Flexural Yield Strength 248.8 MPa
36090 psi
ASTM D790
Flexural Modulus 10.13 GPa
1469 ksi
ASTM D790
Compressive Yield Strength 182.7 MPa
26500 psi
ASTM D695
Izod Impact, Notched 0.840 J/cm
1.57 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.70e+17 ohm-cm
1.70e+17 ohm-cm
ASTM D257
Dielectric Constant 2.1

@Frequency 1e+6 Hz
2.1

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 19.5 kV/mm
495 kV/in
Short Time; ASTM D149
Arc Resistance 120 sec
120 sec
ASTM D495
Comparative Tracking Index 225 V
225 V
ASTM D3638