Polymer Property : CTE, linear = 1.11 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 2.00 µm/m-°C

@Temperature 900 °C
1.11 µin/in-°F

@Temperature 1650 °F
MarkeTech Repton 931 Cordierite Mg-Al-Si Oxide
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa..
CTE, linear 2.00 µm/m-°C

@Temperature 900 °C
1.11 µin/in-°F

@Temperature 1650 °F
MarkeTech Repton EXP 48 Cordierite Mg-Al-Si Oxide
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa..
CTE, linear 2.00 µm/m-°C

@Temperature 1000 °C
1.11 µin/in-°F

@Temperature 1830 °F
"ab" direction
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride
Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi..
CTE, linear 2.00 - 3.00 µm/m-°C

@Temperature 20.0 - 600 °C
1.11 - 1.67 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C373
CeramTec Sikor® S Cordierite
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c..
CTE, linear 2.00 - 4.00 µm/m-°C

@Temperature 20.0 - 1000 °C
1.11 - 2.22 µin/in-°F

@Temperature 68.0 - 1830 °F
CeramTec Sikor® S Cordierite
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c..
CTE, linear 2.00 µm/m-°C

@Temperature 20.0 - 100 °C
1.11 µin/in-°F

@Temperature 68.0 - 212 °F
DIN EN 821-1
CeramTec SL 303 Silicon Nitride, SiAION+SiC
SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i..
CTE, linear 2.00 - 2.70 µm/m-°C

@Temperature 25.0 - 260 °C
1.11 - 1.50 µin/in-°F

@Temperature 77.0 - 500 °F
ATI Allegheny Ludlum AL 36™ Electrical Alloy (Cryogenic and Bimetal) UNS K93600 or UNS K93603
AL 36 alloy is a nickel-iron alloy combining low thermal expansion properties up to about 200°C along with moderately high strength and good toughness down to -235°C, the temperature of liquid hyd..