Polymer Property : CTE, linear = 0.278 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 0.500 µm/m-°C

@Temperature 20.0 °C
0.278 µin/in-°F

@Temperature 68.0 °F
ab direction
Momentive Performance Materials "PG" Pyrolytic Graphite
Pyrolytic Graphite (PG) is a unique form of graphite manufactured by decomposition of a hydrocarbon gas at very high temperature in a vacuum furnace. The result is an ultra-pure product which is ne..
CTE, linear 0.500 µm/m-°C

@Temperature -30.0 - 70.0 °C
0.278 µin/in-°F

@Temperature -22.0 - 158 °F
Schott LITHOSIL-Q Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 0.500 - 1.10 µm/m-°C

@Temperature 25.0 - 93.0 °C
0.278 - 0.611 µin/in-°F

@Temperature 77.0 - 199 °F
ATI Allegheny Ludlum AL 36™ Electrical Alloy (Cryogenic and Bimetal) UNS K93600 or UNS K93603
AL 36 alloy is a nickel-iron alloy combining low thermal expansion properties up to about 200°C along with moderately high strength and good toughness down to -235°C, the temperature of liquid hyd..