Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 462 MPa | 67000 psi | Annealed |
Special Metals Nickel 200 Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us.. |
|||
Tensile Strength, Ultimate | 462 - 531 MPa | 67000 - 77000 psi | |
Eagle Brass 19010 XP-150 Copper Nickel Silicon, 3/4 Hard 19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect.. |
|||
Tensile Strength, Ultimate | 462 - 503 MPa | 67000 - 73000 psi | |
Eagle Brass 194 HSM® Copper, Extra Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Strength, Ultimate | 462 - 565 MPa | 67000 - 82000 psi | |
Eagle Brass 511 Phosphor Bronzes 4%, 3/4 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Ultimate | 462 - 517 MPa | 67000 - 75000 psi | Typical |
AK Steel 18 Cr-Cb™ Ferritic Stainless steel AK Steel 18 Cr-Cb™ provides a more effective solution than Type 409 to many automotive exhaust applications, due to its higher oxidation resistance, improved creep resistance and moderate formabili.. |
|||
Tensile Strength, Ultimate | 462 MPa @Temperature 538 °C |
67000 psi @Temperature 1000 °F |
|
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Tensile Strength, Ultimate | 462 MPa | 67000 psi | Semi-Processed |
AK Steel DI-MAX® M-47 Nonoriented Electrical Steel Nonoriented electrical steels are silicon steels in which magnetic properties are practically the same in any direction of magnetism in the plane of the material. Standard
grades from M-15 to M-47 .. |
|||
Tensile Strength, Ultimate | 462 MPa | 67000 psi | Typical Annealed |
ATI Allegheny Ludlum AL 200™ Nickel Alloy, UNS N02200 Ferromagnetic. Allegheny Ludlum AL 200 alloy is wrought commercially pure nickel. This alloy provides highly ductile mechanical properties across a wide temperature range. Either alloy provides c.. |
|||
Tensile Strength, Ultimate | 462 MPa | 67000 psi | Typical Annealed |
ATI Allegheny Ludlum AL 36™ Electrical Alloy (Cryogenic and Bimetal) UNS K93600 or UNS K93603 AL 36 alloy is a nickel-iron alloy combining low thermal expansion properties up to about 200°C along with moderately high strength and good toughness down to -235°C, the temperature of liquid hyd.. |
|||
Tensile Strength, Ultimate | 462 MPa @Temperature 23.9 °C |
67000 psi @Temperature 75.0 °F |
Annealed, Transverse Orientation |
AK Steel 439 ULTRA FORM® Stainless Steel AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul.. |