Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 2.00 µm/m-°C @Temperature 900 °C |
1.11 µin/in-°F @Temperature 1650 °F |
|
MarkeTech Repton 931 Cordierite Mg-Al-Si Oxide REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
CTE, linear | 2.00 µm/m-°C @Temperature 900 °C |
1.11 µin/in-°F @Temperature 1650 °F |
|
MarkeTech Repton EXP 48 Cordierite Mg-Al-Si Oxide REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
CTE, linear | 2.00 µm/m-°C @Temperature 1000 °C |
1.11 µin/in-°F @Temperature 1830 °F |
"ab" direction |
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi.. |
|||
CTE, linear | 2.00 - 3.00 µm/m-°C @Temperature 20.0 - 600 °C |
1.11 - 1.67 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C373 |
CeramTec Sikor® S Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
CTE, linear | 2.00 - 4.00 µm/m-°C @Temperature 20.0 - 1000 °C |
1.11 - 2.22 µin/in-°F @Temperature 68.0 - 1830 °F |
|
CeramTec Sikor® S Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
CTE, linear | 2.00 µm/m-°C @Temperature 20.0 - 100 °C |
1.11 µin/in-°F @Temperature 68.0 - 212 °F |
DIN EN 821-1 |
CeramTec SL 303 Silicon Nitride, SiAION+SiC SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i.. |
|||
CTE, linear | 2.00 - 2.70 µm/m-°C @Temperature 25.0 - 260 °C |
1.11 - 1.50 µin/in-°F @Temperature 77.0 - 500 °F |
|
ATI Allegheny Ludlum AL 36™ Electrical Alloy (Cryogenic and Bimetal) UNS K93600 or UNS K93603 AL 36 alloy is a nickel-iron alloy combining low thermal expansion properties up to about 200°C along with moderately high strength and good toughness down to -235°C, the temperature of liquid hyd.. |