Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC Stretch Effect QSI Quantum Silicones Stretch Effect 22 Durometer Addition Cure Translucent Moldmaking Material &

Category Polymer , Thermoset , Silicone
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC Stretch Effect QSI Quantum Silicones Stretch Effect 22 Durometer Addition Cure Translucent Moldmaking Material &.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, fast demold time, high elongation, excellent flexibility. Applications: special effects, skin replication, where pigment is required.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Base
Viscosity 20000 cP
20000 cP
catalyzed with Stretch Effect B
25000 cP
25000 cP
Base
Mechanical Properties Metric English Comments
Hardness, Shore A 22
22
cured
Tensile Strength, Yield >= 2.80 MPa
>= 406 psi
cured
Elongation at Break >= 1200 %
>= 1200 %
cured
Tear Strength >= 17.5 kN/m
>= 100 pli
cured
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Dry Time 8 - 12 hour
8 - 12 hour
Demold time, catalyzed with Stretch Effect B
Pot Life >= 90 min
>= 90 min
catalyzed with Stretch Effect B
Descriptive Properties Value Comments
Color Translucent
catalyzed with Stretch Effect B
Translucent
Base
Linear Shrinkage, inches, max 0.1
Users viewing this material also viewed the following: