Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.70 - 44.1 MPa | 247 - 6400 psi | Average value: 11.3 MPa Grade Count:147 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Yield | >= 1.70 MPa | >= 247 psi | catalyzed |
ACC QSil 551 QSI Quantum Silicones Silicone Potting Material
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: 100% solid, long pot life, low modulus, good elongation. |
|||
Tensile Strength, Yield | 1.70 MPa | 247 psi | cured |
ACC QLE 1030 QSI Quantum Silicones 27 Durometer Addition Cure Elastomer for Coating
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: long pot life, excellent adhesion, 100%solid, fast cure.Applications: fabric or cloth coating. Part of the Amber Chem.. |
|||
Tensile Strength, Yield | 1.70 MPa | 247 psi | 508 mm/min; ASTM D638 |
Dow Engage® 8180 Polyolefin Elastomer Description: Engage® 8180 polyolefin elastomer is a lower density, high performance ethylene-octene copolymer that has excellent flow characteristics and provides good impact properties in blends w.. |
|||
Tensile Strength, Yield | 1.70 MPa | 247 psi | |
ACC MM50T Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Tensile Strength, Yield | 1.70 MPa | 247 psi | cured 20 mins @150°C |
ACC QLE 1031 QSI Quantum Silicones 25 Durometer Addition Cure Elastomer for Coating QLE 1031 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |