Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
Polymax® Maxelast® C4912 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
Polymax® Maxelast® C4915 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
Polymax® Maxelast® C4920 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
Polymax® Maxelast® P3915T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
Polymax® Maxelast® P3932C TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
Polymax® Maxelast® P3936C TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
Polymax® Maxelast® C4909 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
Polymax® Maxelast® C4930 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM 792 |
Multibase Multi-Flex® D 6500 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant General PurposeDensity, LowTear Strength, GoodUV Resistance, Good Forms:PelletsProcessing Method:Blow Molding Uses: Automotive Applica.. |
|||
Specific Gravity | 0.882 - 0.888 g/cc | 0.882 - 0.888 g/cc | Hydrometer; ASTM D1298 |
LG Chemical 2-Ethyl Hexyl Acrylate Features: Low Color- Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity -Through the multistage .. |
|||
Specific Gravity | 0.882 - 0.886 g/cc | 0.882 - 0.886 g/cc | ASTM D3505 |
LG Chemical Benzene Physical Properties: Bright and colorless liquid, Unique odor (Low density) and Unpleasant smell (High density) Structure & Characteristics: CH2=CH2. A colorless inflammable liquefied gas which ha.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2235 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
Teknor Apex Monprene® MP-2676 UV Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D4052 |
ExxonMobil Mobil Aero HFA Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D792 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | |
Dow Corning 1-6136 ANTISTAT Dow Corning 1-6136 Antistat is a cationic alkoxy silane and is designated 3-trimethoxysilylpropyloctadecyidimethyl ammonium chloride. It is supplied as a 42 percent active solution (by weight) in me.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | 60°F |
ConocoPhillips El Mar® 3000 Oil SAE Grade 15W-40 Description: Conoco El Mar® 3000 Oil is a quality, low ash gas engine oil recommended for naturally aspirated and moderately turbocharged, four cycle, low-, medium- and high-speed gas engines, such.. |
|||
Specific Gravity | 0.882 g/cc | 0.882 g/cc | ASTM D4052 |
ExxonMobil Mobil Aero HFA Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |