A. Schulman POLYBATCH™ MAS-25 Concentrate Based In LDPE

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBATCH™ MAS-25 Concentrate Based In LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBATCH® MAS-25 is an organic antislip concentrate based in LDPE. This masterbatch is designed for use in moderate to heavy gauge film and sheet applications where extreme antislip properties are required. POLYBATCH® MAS-25 is typically used at 3 to 5% loading levels depending upon customer specific application requirements. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Descriptive Properties Value Comments
Moisture 1000
ppm, ASTM D789 @ 190°C
Pellet Count 70
pellets/gram