Material Notes:
DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. ApplicationFormion® FI 226 is targeted for non painted, mold-in-color, exterior or interior appearance applications. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ISO 1183/1
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm

@Thickness 3.20 mm
0.00050 - 0.0015 in/in

@Thickness 0.126 in
72 hr; ISO 294
Mechanical Properties Metric English Comments
Tensile Strength, Yield 97.0 MPa
14100 psi
ISO 527
Elongation at Break 4.0 %
4.0 %
ISO 527
Flexural Modulus 7.95 GPa
1150 ksi
Tangent; ISO 178
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) >= 195 °C

@Thickness 3.20 mm
>= 383 °F

@Thickness 0.126 in
ISO 75