Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Thanecure ZM

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Thanecure ZM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.FormulationMillathane E34100.0N330 Black30.0Cumar P1010.0MBTS4.0MBT2.0Sulfur1.5Zinc Stearate0.5Thanecure® ZM3.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A >= 66
>= 66
Tensile Strength, Yield 30.23 MPa
4384 psi
Elongation at Yield 500 %
500 %
100% Modulus 0.00340 GPa
0.493 ksi
200% Modulus 0.007598 GPa
1.102 ksi
300% Modulus 0.01290 GPa
1.871 ksi
Tear Strength 40.8 kN/m
233 pli
Die C
Compression Set 33.4 %

@Temperature 70.0 °C,
Time 79200 sec
33.4 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 8.00 min

@Temperature 68.3 °C
0.133 hour

@Temperature 155 °F
Copyright © lookpolymers.com All Rights Reserved