Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman CP814-01 Linear, Low-Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman CP814-01 Linear, Low-Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA Regulation CFR 177.1520(c)3.1.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.924 g/cc
0.924 g/cc
ASTM D792
ESCR 100% Igepal® 50 hour
50 hour
Condition C; ASTM D1692
Melt Index of Compound 50 g/10 min
50 g/10 min
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D2240
Tensile Strength, Yield 11.0 MPa
1600 psi
2"/min; ASTM D638
Elongation at Break 175 %
175 %
2"/min; ASTM D638
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Brittleness Temperature -71.0 °C
-95.8 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 122 °C
252 °F
Users viewing this material also viewed the following: