Polymer Property : Melt Index of Compound = 50 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 50 g/10 min

@Load 5.00 kg,
Temperature 260 °C
50 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Polykemi AB POLYblend C65F PC/ABS-blend
Information provided by Polykemi AB
Melt Index of Compound 50 g/10 min

@Load 5.00 kg,
Temperature 260 °C
50 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Polykemi AB POLYblend C65HF PC/ABS-blend
Information provided by Polykemi AB
Melt Index of Compound 50 g/10 min

@Load 10.0 kg,
Temperature 190 °C
50 g/10 min

@Load 22.0 lb,
Temperature 374 °F
MVR, [cm<sup>3</sup>/10 min]
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester
Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti..
Melt Index of Compound 50 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50 g/10 min

@Load 47.6 lb,
Temperature 374 °F
cm<sup>3</sup>/10 min
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec..
Melt Index of Compound 50 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50 g/10 min

@Load 47.6 lb,
Temperature 374 °F
MVR, [cm<sup>3</sup>/10 min]
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester
Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig..
Melt Index of Compound 50 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50 g/10 min

@Load 47.6 lb,
Temperature 374 °F
cm<sup>3</sup>/10 min
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether
Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th..
Melt Index of Compound 50 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50 g/10 min

@Load 47.6 lb,
Temperature 374 °F
cm<sup>3</sup>/10 min
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether
Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th..
Melt Index of Compound 50 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50 g/10 min

@Load 47.6 lb,
Temperature 374 °F
cm<sup>3</sup>/10 min
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi..
Melt Index of Compound 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ICO Polymers ICOFLOâ„¢ 510-5028 400 Micron LLDPE Powder
Description: ICOFLO 510-5028 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Melt Index of Compound 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ICO Polymers ICOFLOâ„¢ 510-5073 500 Micron LLDPE Powder
Description: ICOFLO 510-5073 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Melt Index of Compound 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ICO Polymers ICOFLOâ„¢ 510-5074 800 Micron LLDPE Powder
Description: ICOFLO 510-5074 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Melt Index of Compound 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ICO Polymers ICOFLOâ„¢ 510-5075 1200 Micron LLDPE Powder
Description: ICOFLO 510-5075 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Melt Index of Compound 50 g/10 min

@Load 21.6 kg,
Temperature 190 °C
50 g/10 min

@Load 47.6 lb,
Temperature 374 °F
cm<sup>3</sup>/10 min
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo..
Melt Index of Compound 50 g/10 min

@Load 5.00 kg,
Temperature 315 °C
50 g/10 min

@Load 11.0 lb,
Temperature 599 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics LNP LUBRICOMP OCL13XXP PPS - LINEAR (Europe-Africa-Middle East)
LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Melt Index of Compound 50 g/10 min

@Load 10.0 kg,
Temperature 300 °C
50 g/10 min

@Load 22.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific)
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..
Melt Index of Compound 50 g/10 min

@Load 10.0 kg,
Temperature 300 °C
50 g/10 min

@Load 22.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East)
LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, ..
Melt Index of Compound 50 g/10 min
50 g/10 min
Condition E; ASTM D1238
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Melt Index of Compound 50 g/10 min
50 g/10 min
Condition E; ASTM D1238
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Melt Index of Compound 50 g/10 min
50 g/10 min
Condition E; ASTM D1238
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Melt Index of Compound 50 g/10 min
50 g/10 min
Condition E; ASTM D1238
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Melt Index of Compound 50 g/10 min
50 g/10 min
Condition E; ASTM D1238
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Melt Index of Compound 50 g/10 min
50 g/10 min
Condition E; ASTM D1238
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Melt Index of Compound 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-7147 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as food containers, housewares and lids. Information provided by D..
Melt Index of Compound 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE)
DOWLEX™ IP-51 is an Improved Processing high density resin designed to offer excellent process-ability and impact performance. This resin was designed by optimization of the breadth, shape and pea..
Melt Index of Compound 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Dow R7021-50RNA Polypropylene Random Copolymer Resin
DOW™ R7021-50RNA Polypropylene Resin is a random copolymer designed for thin wall injection molding applications desiring high clarity.Main CharacteristicsGood impact propertiesExcellent opticsFast..