Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Falling Dart Impact = 20.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Falling Dart Impact 27.1 J
20.0 ft-lb
73°F; ASTM D3029
Spartech SolarKote® /ABS Weatherable Sheet
Description: Weatherable SheetSolarKote is a registered trademark of Atofina Chemicals, Inc..Information provided by Spartech.
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM D3029
Spartech SP-9070 ABS/PVC Flame Retardant Sheet
Description: Flame Retardant SheetInformation provided by Spartech.
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM 3029
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM D5420
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM 3029
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM D5420
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM 3029
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM 3029
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM D5420
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM 3029
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM D5420
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM D5420
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM D5420
A. Schulman CP814-01 Linear, Low-Density Polyethylene
DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA ..
Falling Dart Impact 27.1 J

@Temperature -40.0 °C
20.0 ft-lb

@Temperature -40.0 °F
ASTM 3029
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Copyright © lookpolymers.com All Rights Reserved