Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact streng.. |
|||
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Melt Temperature | 122 °C | 252 °F | |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |