3M Scotchkote™ KSIR88 Epoxy Coating

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ KSIR88 Epoxy Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Scotchkote Epoxy Coating KSIR88 has been specifically developed as a high performance solvent based coating for pumps, valves fittings, tanks, and pipelines. Scotchkote epoxy coating KSIR88 combines good application characteristics with excellent corrosion protection and chemical resistance.Information provided by 3M
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Solids Content 60 %
60 %
Volatile Organic Compounds (VOC) Content 350 g/l
350 g/l
as supplied
393 g/l
393 g/l
thinned 10%
Thickness 125 microns
4.92 mil
Processing Properties Metric English Comments
Cure Time 60.0 min
1.00 hour
Touch Dry
480 min
8.00 hour
Hard Dry
10100 min
168 hour
Full Cure
Shelf Life 24.0 Month

@Temperature 5.00 - 32.0 °C
24.0 Month

@Temperature 41.0 - 89.6 °F
Descriptive Properties Value Comments
Appearance Off White, Light Gray and Blue