3M Scotch-Weld™ EC600 General Purpose Instant Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ EC600 General Purpose Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, metals, and other common substrates. They are available in a wide variety of viscosities. Higher viscosity to reduce migration form bond area.Information provided by 3M
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Uncured
Viscosity 600 cP
600 cP
Brookfield Viscosity 500 - 700 cP
500 - 700 cP
LVF sp #2 @30 rpm
Mechanical Properties Metric English Comments
Shear Strength 20.7 MPa
3000 psi
cured, grit-blasted steel; ASTM D1002
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.0833 - 1.00 min
0.00139 - 0.0167 hour
Time to Handling Strength
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear liquid