Polymer Property : Brookfield Viscosity = 500 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 500 cP
500 cP
One Day Viscosity @ 6rpmGeon® STP 1434 (with provided formulation); Internal Method
PolyOne Geon™ 170 Series 174 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 174 is a medium molecular weight, fine particle size homopolymer dispersion resin. It provides a good balance of fused film properties and processing temperatures. It is recommended for appli..
Brookfield Viscosity <= 500 cP
<= 500 cP
#2/20 rpm
Mallard Creek Polymers PolySaf® 5600 Cationic Polymer
PolySaf® 5600 polymer provides exceptional deodorancy performance in personal care products. This non-irritating cationic polymer also enhances the sensory performance of body washes.Markets: Per..
Brookfield Viscosity <= 500 cP
<= 500 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 4049 SBR Latex
ROVENE® 4049 is a carboxylated styrene-butadiene emulsion that has a medium hand with above average strength properties. This binder has the ability to be cross-linked with external cross-linking..
Brookfield Viscosity <= 500 cP
<= 500 cP
#20/200
Mallard Creek Polymers Rovene® 4111 Styrene-Butadiene Emulsion
Rovene® 4111 was designed with a specific particle size that greatly improves the spacing between titanium dioxide particles resulting in increased opacity. Additionally, using Rovene® 4111 ma..
Brookfield Viscosity <= 500 cP
<= 500 cP
#20/200
Mallard Creek Polymers Rovene® 6065 Styrene-Acrylic Emulsion
Applications: Rovene® 6065 is a tough, durable nonwoven binder intended to provide improved stiffness and strength. Rovene® 6065 was specifically designed to perform in formaldehyde-free syste..
Brookfield Viscosity 500 - 1800 cP
500 - 1800 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 6101 Styrene-Acrylic Emulsion
ROVENE® 6101 is a stiff, non-film forming high-gloss extending vehicle for flexographic and gravure inks and overprint varnishes. It is intended for use primarily on paper and paperboard.APPLICAT..
Brookfield Viscosity 500 - 1800 cP
500 - 1800 cP
#20/200
Mallard Creek Polymers Rovene® 6103 Resin Supported Emulsion
Rovene® 6103 is a soft, film forming vehicle that provides good water and rub resistance for flexographic and gravure inks and overprint varnishes. Rovene® 6103 can be used as the film forming..
Brookfield Viscosity <= 500 cP
<= 500 cP
#20/200
Mallard Creek Polymers Rovene® 6119 Styrene-Acrylic Emulsion
Applications: Rovene® 6119 is a low glass transition temperature styrene-acrylic polymer that offers flexibility during movement of the substrate and water resistance. Rovene® 6119 also exhibi..
Brookfield Viscosity <= 500 cP
<= 500 cP
#20/200
Mallard Creek Polymers Rovene® 6506 Styrene-Acrylic Emulsion
Applications: Rovene® 6506 typical applications are across a variety of nonwoven markets and substrates. Rovene® 6506 has demonstrated excellent performance as a binder on a lightweight nonwov..
Brookfield Viscosity <= 500 cP
<= 500 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 97982 Acrylic Emulsion
ROVENE® 97982 is a very soft acrylic latex emulsion suggested as a base resin in flexible packaging laminating adhesives. Rovene® 97982 provides formulations with excellent clarity and UV stab..
Brookfield Viscosity 500 - 1700 cP
500 - 1700 cP
Spindle # 3, rpm 60
Michelman® Hydrosize® U2022 Nonionic polyurethane emulsion
Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2022 is an APE free, high strength sizing for glass and carbon chopped fiber, with excellent adhesion.Information provided by Michelm..
Brookfield Viscosity <= 500 cP
<= 500 cP
Spindle # 2, rpm 60
Michelman® Michem® Emulsion 27720 Nonionic slip and anti-block additive
Description: Nonionic slip and anti-block additiveUsage: Michem® Emulsion 27720 is a nonionic, amide emulsion used for anti-blocking, slip and mar resistant properties.We serve many markets throu..
Brookfield Viscosity <= 500 cP
<= 500 cP
Spindle # 3, rpm 60
Michelman® Michem® Emulsion 48625M1 Polymer solution
Description: Polymer solutionUsage: Michem® Emulsion 48625M1 is a sizing polymer for fiberglass and other fibers serving as reinforcement for various resins.We serve many markets through MichemÂ..
Brookfield Viscosity <= 500 cP
<= 500 cP
Spindle # 3, rpm 60
Michelman® Michem® Flex P1801 Water based primer
Description: Water based primer for liquids and extrusion coated resins.Usage: Michem®Flex P1801 is a primer for film and paper substrates to promote adhesion to extrusion coated resins resulting..
Brookfield Viscosity <= 500 cP
<= 500 cP
Spindle # 3, rpm 60
Michelman® Michem® Guard 7140 Anionic dispersion of polyethylene wax
Description: Anionic dispersion of polyethylene waxUsage: Michem® Guard 7140 is a water-based, large particle emulsion which improves rub and abrasion resistance in pigmented coatings and semi-gl..
Brookfield Viscosity <= 500 cP
<= 500 cP
Spindle # 2, rpm 60
Michelman® Michem® Prime 2960 Ethylene acrylic acid dispersion
Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 2960 provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent re..
Brookfield Viscosity <= 500 cP
<= 500 cP
Spindle # 2, rpm 60
Michelman® Michem® Wood Coating 70M Anionic paraffin blend emulsion
Description: Anionic paraffin blend emulsionUsage: Michem® Wood Coating 70M is a high solids, water resistant topical wood treatment for exterior wood and wood composites. It provides good water ..
Brookfield Viscosity 500 cP

@Temperature 25.0 °C
500 cP

@Temperature 77.0 °F
25% Toluene solution; BAM 922
Kraton® D1117 P (SIS) Linear Block Copolymer
Description:Kraton D1117 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 17%. It is supplied from North America in the physical form identified: K..
Brookfield Viscosity 500 cP

@Temperature 25.0 °C
500 cP

@Temperature 77.0 °F
20 RPM
KaMin Hydralux® 91 Clay
Hydralux® 91 is a high brightness, fine glossing coating clay used in heavy weight coated paper and coated board application. Its fine particle excellent flow properties and size allow for high ..
Brookfield Viscosity 500 cP

@Temperature 25.0 °C
500 cP

@Temperature 77.0 °F
20 RPM
KaMin KaMin® Tek 2001 Clay
The uniform, narrow particle size distribution and excellent color makes Kamin® TEK 2001 the preferred extender for gloss latex paints where optimum TiO2 spacing is desired without adverse effect..
Brookfield Viscosity 500 - 1000 cP
500 - 1000 cP
Spindle # 3, rpm 60
Michelman® Michem® Guard 60 Nonionic Fischer-Tropsch dispersion
Description: Nonionic Fischer-Tropsch dispersionUsage: Michem® Guard 60 is a dispersion which provides mar resistance properties when used as an additive in paint, coating, ink and graphic art fo..
Brookfield Viscosity 500 - 1100 cP
500 - 1100 cP
Brookfield RVF sp 3, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Lubrizol Advanced Materials Pearlstick® D40-70/08 Linear Thermoplastic Polyurethane
Pearlstick D40-70/08 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. S..
Brookfield Viscosity 500 cP
500 cP
30 rpm
Solvay RHODOLINE® 581B Surfactant
Description: Mineral oil defoamers for high PVC systems Chemical Name: DEFOAMERCAS: 64742-47-8Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility(2% in DI Water): Coarse Di..
Brookfield Viscosity 500 cP

@Temperature 25.0 °C
500 cP

@Temperature 77.0 °F
Loctite® 4981 Cyanoacrylate Adhesive
Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe..
Brookfield Viscosity 500 - 700 cP

@Temperature 25.0 °C
500 - 700 cP

@Temperature 77.0 °F
C.O.I.M. EXTER S® S 501 Neopentylic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 501: Resin for high-..
Brookfield Viscosity 500 - 700 cP

@Temperature 25.0 °C
500 - 700 cP

@Temperature 77.0 °F
C.O.I.M. EXTER S® S 801 Neopentylic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 801: Resin for gel-c..
Brookfield Viscosity 500 - 2500 cP
500 - 2500 cP
RVF #6 sp. @ 4 rpm
3M Scotch-Seal™ 1252 Tamper Proof Sealant
3M™ Scotch-Seal™ Tamper Proof Sealant 1252 is a fast drying, anti-tamper sealer which is fire retardant.Features: Can be applied over adjustable or removable parts to indicuate changes in adjustme..
Brookfield Viscosity 500 - 700 cP
500 - 700 cP
LVF sp #2 @30 rpm
3M Scotch-Weld™ EC600 General Purpose Instant Adhesive
3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me..
Brookfield Viscosity 500 cP
500 cP
#1 spindle; 30 rpm.
DuPont Performance Polymers Neoprene 115 Polychloroprene  (discontinued **)
Main feature: Mechanical stability methacrylic acid copolymer reactive. Principal uses include: Coatings, Modifiers, Asphalt, Concrete.Solids content: 47%. Initial pH: 7. Surface tension: 47 dyne..
Brookfield Viscosity 500 cP
500 cP
DuPont Performance Polymers AquaStik® AQS-1120 Polychloroprene Latex  (discontinued **)
Aquastik™ polychloroprene latexes have been designed for the adhesives industry. They provide an environmentally friendly alternative to solvent-borne systems.This grade features mechanical stabil..