Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.89 MPa | 1000 psi | Across flow; ASTM D412 |
ExxonMobil Santoprene® 8291-65TB Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer which bonds to adhesive/epoxy spin-finished polyester or standard nylon fibers for closed-braid hose and woven-substrate products. With bonds strong.. |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | 510 mm/min; ASTM D412A |
PolyOne Synprene® RT-3770 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D638 |
LyondellBasell Microthene® G MN71400 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D1414 |
Greene Tweed Xyfluor® 860 Fluorinated Elastomer Compound Xyfluor® 860, a highly fluorinated elastomer compound, offers excellent chemical compatibility over a wide range of temperatures from -76°F to 450°F (-60°C to 232°C). Recommended for.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP 9000 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP-1458 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP-1518C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP-1766B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP-1862R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP-2024A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP-2132 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP 1544 Thermoplastic Elastomer Notes: Translucent Features: Good Chemical and Oil ResistanceInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP-1876 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP-2634A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Telcar® TL-2433A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | 20 in/min at 23°F; ASTM D412 |
Teknor Apex Telcar® TL-88-N882-A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Telcar® TL-91-T3056D-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | >= 6.89 MPa | >= 1000 psi | |
Master Bond EP37-3FLSP Optically Clear Epoxy Has Low Exotherm Description: Master Bond EP37-3FLSP is a very flexible, low viscosity, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. It fe.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ISO 527-2/1A/50 |
ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade) Product Description: LD 654 is a very high flow LDPE grade with a very good flexibility. It can be added to low-flowing LDPE grades to improve their processability.Availability: Africa & Middle East.. |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | ASTM D412 |
3M Scotch® 70 HDT Self-Fusing Silicone Rubber Electrical Tape with Tapered Edge Scotch® Silicone Rubber Electrical Tape 70 HDT is a high-temperature arc-and track-resistant tape composed of self-fusing, inorganic silicone rubber and easy-tear and easy-strip liner. The 70 HDT p.. |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | |
3M Scotchkote™ 60FG 534 Urethane Elastomer Scotchkote Urethane Elastomer 60FG 534 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components.Product Features:Physical properti.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP-2890M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Compuestos Dominicanos Polycom CH-550140 PVC Compound Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist.. |
|||
Tensile Strength at Break | 6.89 MPa | 1000 psi | ASTM D412 |
Teknor Apex Monprene® MP-2785H Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |