Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.89 MPa | 999 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-2065 Thermoplastic Polyolefin Elastomer (TPO (POE)) PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o.. |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D6500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C6501 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | 510 mm/min; ASTM D412A |
PolyOne Synprene® RT-3770 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | ASTM D412 |
3M Scotch® 70 HDT Self-Fusing Silicone Rubber Electrical Tape with Tapered Edge Scotch® Silicone Rubber Electrical Tape 70 HDT is a high-temperature arc-and track-resistant tape composed of self-fusing, inorganic silicone rubber and easy-tear and easy-strip liner. The 70 HDT p.. |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | ASTM D1000 |
3M Scotch® 70 Self-Fusing Silicone Rubber Electrical Tape Scotch® 24 Brand 70 Silicone Rubber Electrical Tape is a high-temperature arc and track resistance tape composed of self-fusing, inorganic silicone rubber and easy-tear and easy-strip liner.Informa.. |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | |
3M Scotchkote™ 80FG 532 Urethane Elastomer Scotchkote Urethane Elastomer 80FG 532 has been specifically developed as an elastomeric system with a high degree of flexibility for casting and molding rubber components.Product Features:Propertie.. |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | 50% RH |
3M 5200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds with excellent adhesion to wood and fiberglass. Forms watertight, weather-resistant seals .. |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | |
3M Scotchkote™ 60EG 533 Urethane Elastomer Scotchkote Urethane Elastomer 60EG 533 has been specifically developed as an elastomeric repair system with a high degree of flexibility for rebuilding and resurfacing rubber components.Product Feat.. |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | |
3M Scotchkote™ 60FG 534 Urethane Elastomer Scotchkote Urethane Elastomer 60FG 534 has been specifically developed as an elastomeric system with a high degree of flexibility for resurfacing rubber components.Product Features:Physical properti.. |
|||
Tensile Strength at Break | 6.89 MPa | 999 psi | Solvent Resistance |
3M TMW Tubing 3M TMW Tubing is a semi-rigid translucent heat-shrinkable polyolefin tubing that is co-extruded and selectively cross-linked with an integral, meltable inner wall. When heated in excess of 135°C th.. |