Material Notes:
3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesive P1655 OW, which is a high performance white permanent tackified acrylic adhesive designed for use in demanding environments, including automotive applications. This adhesive offers excellent opacity and adhesion to a wide variety of substrates.Information provided by 3M
Physical Properties Metric English Comments
Thickness 27.9 microns
1.10 mil
Adhesive
58.4 microns
2.30 mil
Facestock
78.7 microns
3.10 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.789 kN/m
4.50 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Application
60.0 °C
140 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
5.00 °C
41.0 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type P1655 OW
Liner 50# SC