Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 58.4 microns | 2.30 mil | |
3M 941 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Thickness | 58.4 microns | 2.30 mil | Backside Adhesive |
3M 9500B Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Thickness | 58.4 microns | 2.30 mil | Faceside Adhesive |
3M 9500PC Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Thickness | 58.4 microns | 2.30 mil | Backside Adhesive |
3M 9500PC Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 9502 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 965 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thickness | 58.4 microns | 2.30 mil | Adhesive |
3M 9671LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Thickness | 58.4 microns | 2.30 mil | Faceside Adhesive |
3M 9832 Double Coated Tapes with Adhesive 300MP 3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP012202 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP012603 White Polyester Label Products ion 3M™ White Polypropylene Label Products are glossy white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP022202 White Polypropylene Label Products 3M™ White Polypropylene Label Products FP022202 is a white opaque material that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480, which is a high.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP024509 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3800, which is an ultra removable acrylic designed t.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP031105 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP032302 White Metallized Polypropylene Label Products 3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesi.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP032302W White Metallized Polypropylene Label Products 3M™ White Metallized Polypropylene Label Products FP032302, FP032302W and FP032305 are a white opaque material that offers excellent durability and opacity. These label products utilize 3M™ Adhesi.. |
|||
Thickness | 58.4 microns | 2.30 mil | Total; ASTM D3652 |
3M Scotch® 600 Transparent Film Tape Scotch® Tape 600 is a transparent film tape that is excellent for various packaging applications. It has a pressure sensitive acrylic adhesive system which is long aging and highly transparent, so .. |
|||
Thickness | 58.4 microns | 2.30 mil | Total; ASTM D3652 |
3M Scotch® 610 Cellophane Film Tape Scotch® Cellophane Film Tape 610 is a high performance, transparent cellophane film tape featuring a high tack adhesive system. This product offers excellent adhesion, dispensing and handling prope.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M 7880 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Material 7880 is a 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for traditional.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thickness | 58.4 microns | 2.30 mil | Adhesive |
3M 8132LE Adhesive Transfer Tapes with Adhesive 300LSE 3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p.. |
|||
Thickness | 58.4 microns | 2.30 mil | Total; ASTM D3752 |
3M 8911 Polyester Tape 3M™ Polyester Tape 8911 is a transparent polyester tape with silicone adhesive that can be used in composite bonding, splicing, and applications that may require high temperature, chemical, and abr.. |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 9552 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FP016903 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Thickness | 58.4 microns | 2.30 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
Thickness | 58.4 microns | 2.30 mil | |
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thickness | 58.4 microns | 2.30 mil | Facestock |
3M FV022702 White Vinyl Label Products 3M™ White Vinyl Label Products FV022702 and FV022705 are flexible and conformable materials that offer durability and moisture resistance. The polymerically plasticized nature of this soft flexible.. |