3M Dyneon™ TFM™ 4105 Modified PTFE, 25% Glass Fiber Filled  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TFM™ 4105 Modified PTFE, 25% Glass Fiber Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon.
Physical Properties Metric English Comments
Density 2.24 g/cc
0.0809 lb/in³
Sintered moldings; ASTM D4894/D4895
Apparent Bulk Density 0.820 g/cc
0.0296 lb/in³
DIN 53 466
Linear Mold Shrinkage 0.023 cm/cm

@Thickness 80.0 mm
0.023 in/in

@Thickness 3.15 in
sheet; ASTM D4894
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Ultimate 16.0 MPa

@Thickness 2.00 mm
2320 psi

@Thickness 0.0787 in
ASTM D4894
Elongation at Break 400 %

@Thickness 2.00 mm
400 %

@Thickness 0.0787 in
ASTM D4894
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 30.0 - 100 °C
50.0 µin/in-°F

@Temperature 86.0 - 212 °F
110 µm/m-°C

@Temperature 30.0 - 200 °C
61.1 µin/in-°F

@Temperature 86.0 - 392 °F
130 µm/m-°C

@Temperature 30.0 - 300 °C
72.2 µin/in-°F

@Temperature 86.0 - 572 °F
Thermal Conductivity 0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
DIN 52 612
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093