Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | DIN 53 466 |
3M Dyneon™ TFM™ 1605 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Second-generation PTFE that is a chemically modified to allow new designs and processing methods. Very good free-flowing powder properties.Data provided by Dyneon. |
|||
Apparent Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | ASTM D4894 |
3M Dyneon™ TF 4103 PTFE 15% Glass Fiber Filled
(discontinued **) Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon. |
|||
Apparent Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | DIN 53 466 |
3M Dyneon™ TF 4105 PTFE 25% Glass Fiber Filled
(discontinued **) Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon. |
|||
Apparent Bulk Density | 0.820 g/cc | 0.0296 lb/in³ | DIN 53 466 |
3M Dyneon™ TFM™ 4105 Modified PTFE, 25% Glass Fiber Filled
(discontinued **) Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon. |