Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Elastoblend® PA6 GF30 IM L 30% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled , Nylon 6, Impact Grade
Manufacturer Techmer ES
Trade Name Elastoblend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Elastoblend® PA6 GF30 IM L 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File Number: E157318Processing Method: Injection MoldingInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.035 cm/cm

@Thickness 3.17 mm
0.035 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 152 MPa
22000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
1.90 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
1.66 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
3.10 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Izod Impact, Unnotched 13.9 J/cm

@Thickness 3.17 mm
26.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 36.0 µm/m-°C
20.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 213 °C
415 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Dielectric Strength 15.4 kV/mm
390 kV/in
Method A (Short-Time); ASTM D149
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved