Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill® PEEK CF30 HF 30% Carbon Filled

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PEEK CF30 HF 30% Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.14 %

@Time 86400 sec
0.14 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Thickness 3.17 mm
0.0010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 214 MPa
31000 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Flexural Strength 248 MPa
36000 psi
ASTM D790
Flexural Modulus 15.9 GPa
2300 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm
1.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.8 µm/m-°C
6.00 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 288 °C
550 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
ASTM D257
Copyright © lookpolymers.com All Rights Reserved