Polymer Property : Volume Resistivity = 1000 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm

@Temperature 90.0 °C
1000 ohm-cm

@Temperature 194 °F
ISO 3915
Borealis LE0511 Polyethylene Compound, Crosslinkable, Semiconductive
LE0511 is a crosslinkable black polyethylene compound, specially designed for strippable semi conductive screen applications. Applications: LE0511 is intended for strippable outer semi conductive s..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ISO 3915
Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive
LE0563 is a thermoplastic semi conductive compound specifically designed for medium- and high voltage cable systems requiring improved grounding. It may be used either as a complete jacket or as a t..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ISO 3915
Borealis LE0592 Polyethylene
LE0592 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. Applications: LE0592 is intended for semi conductive applications in XLPE m..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ISO 3915
Borealis Supersmooth™ LE0550 Polyethylene Insulation Compound, Crosslinkable
Supersmooth™ LE0550 is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Applications: Supersmooth™ LE0550 is intended for semiconduct..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ISO 3915
Borealis Supersmooth™ LE0592S Polyethylene
Supersmooth™ LE0592S is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Supersmooth™ LE0592S is intended for semiconductive applicat..
Volume Resistivity 1000 ohm-cm

@Temperature 500 °C
1000 ohm-cm

@Temperature 932 °F
CeramTec Sikor® E Cordierite
Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ASTM D257
Trelleborg Horda Cable E6352-A2 Bonded Semiconductive Shielding And Conductor Screen
E6352-A2 is a crosslinkable semiconductive compound based on ethylene copolymer compound, designed for conductor screen and insulation shield applications in XLPE and EPDM insulated cables with bond..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E6352-A2 Bonded Semiconductive Shielding And Conductor Screen
E6352-A2 is a crosslinkable semiconductive compound based on ethylene copolymer compound, designed for conductor screen and insulation shield applications in XLPE and EPDM insulated cables with bond..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E7355-A4 Strippable Semiconductive Shielding
E7355-A4 is a silane crosslinkable, strippable semiconductive compound for medium voltage cables.E7355-A4 meets the requirements as below, when optimal processing, extrusion and crosslinking procedu..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ASTM D257
Trelleborg Horda Cable E8400 Easy Strippable Semiconductive Shielding
E8400 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8400 meets the requirements as be..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E8400 Easy Strippable Semiconductive Shielding
E8400 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8400 meets the requirements as be..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E8406 Easy Strippable Semiconductive Shielding
E8406 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8406 meets the requirements as be..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ASTM D257
Trelleborg Horda Cable E8409 Easy Strippable Semiconductive Shielding
E8409 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8409 meets the requirements as be..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E8409 Easy Strippable Semiconductive Shielding
E8409 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8409 meets the requirements as be..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E8413 Easy Strippable Semiconductive Shielding
E8413 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8413 meets the requirements as be..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E8415 Easy Strippable Semiconductive Shielding
E8415 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8415 meets the requirements as bel..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ASTM D257
Trelleborg Horda Cable E8502 Strippable Semiconductive Shielding
E8502 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8502 meets the requirements as bel..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E8502 Strippable Semiconductive Shielding
E8502 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8502 meets the requirements as bel..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ASTM D257
Trelleborg Horda Cable E8551 Strippable Semiconductive Shielding
E8551 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8551 meets the requirements as bel..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ASTM D257
Trelleborg Horda Cable E8560 Strippable Semiconductive Shielding
E8560 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8560 meets the requirements as bel..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E8560 Strippable Semiconductive Shielding
E8560 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8560 meets the requirements as bel..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ASTM D257
Trelleborg Horda Cable E8561 Strippable Semiconductive Shielding
E8561 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8561 meets the requirements as bel..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ASTM D257
Trelleborg Horda Cable E8900 Strippable Semiconductive Shielding
E8900 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8900 meets the requirements as be..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E8900 Strippable Semiconductive Shielding
E8900 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8900 meets the requirements as be..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ASTM D257
Trelleborg Horda Cable E7310 Bonded Insulation Shielding And Conductor Screen
E7310 is a silane crosslinkable semiconductive compound for medium voltage cables. The material is designed as a conductor screen and bonded insulation shielding.E7310 meets the requirements as bel..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E7310 Bonded Insulation Shielding And Conductor Screen
E7310 is a silane crosslinkable semiconductive compound for medium voltage cables. The material is designed as a conductor screen and bonded insulation shielding.E7310 meets the requirements as bel..
Volume Resistivity <= 1000 ohm-cm

@Temperature 120 °C
<= 1000 ohm-cm

@Temperature 248 °F
ASTM D257
Trelleborg Horda Cable E8465 Easy Strippable Semiconductive Shielding
E8551 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8551 meets the requirements as bel..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
DC; ISO 3915
Borealis LE7704 Polyethylene Compound, Semiconductive, Thermoplastic
LE7704 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7704 is intended for semiconductive applications in medium voltage..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
DC; ISO 3915
Borealis LE7710 Polyethylene Compound, Semiconductive, Thermoplastic
LE7710 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7710 is intended for semiconductive applications in medium voltage ..
Volume Resistivity <= 1000 ohm-cm

@Temperature 90.0 °C
<= 1000 ohm-cm

@Temperature 194 °F
ISO 3915
Borealis Supersmooth™ LE8280 Polyethylene Insulation Compound, Crosslinkable
Supersmooth™ LE8280 is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Applications: Supersmooth™ LE8280 is intended for semiconduct..