Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ISO 3915 |
Borealis LE0516 Polyethylene Compound, Crosslinkable, Semiconductive LE0516 is a crosslinkable black polyethylene compound, specially designed for strippable semi conductive screen applications. Applications: LE0516 is intended for strippable outer semi conductive s.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ISO 3915 |
Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive LE0563 is a thermoplastic semi conductive compound specifically designed for medium- and high voltage cable systems requiring improved grounding. It may be used either as a complete jacket or as a t.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ISO 3915 |
Borealis LE0574 Polyethylene LE0574 is a thermoplastic black polyethylene compound, specially designed for strippable semi conductive screen applications. It can be used in thermoplastic form or crosslinked via a grafting proce.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ISO 3915 |
Borealis LE0592 Polyethylene LE0592 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. Applications: LE0592 is intended for semi conductive applications in XLPE m.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ISO 3915 |
Borealis Supersmooth™ LE0592S Polyethylene Supersmooth™ LE0592S is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Supersmooth™ LE0592S is intended for semiconductive applicat.. |
|||
Volume Resistivity | 1000 ohm-cm @Temperature 20.0 °C |
1000 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec Rocar® S Silicon Carbide, SSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Volume Resistivity | 1000 ohm-cm @Temperature 500 °C |
1000 ohm-cm @Temperature 932 °F |
|
CeramTec Sikor® E Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ASTM D257 |
Trelleborg Horda Cable E6352-A2 Bonded Semiconductive Shielding And Conductor Screen E6352-A2 is a crosslinkable semiconductive compound based on ethylene copolymer compound, designed for conductor screen and insulation shield applications in XLPE and EPDM insulated cables with bond.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E6352-A2 Bonded Semiconductive Shielding And Conductor Screen E6352-A2 is a crosslinkable semiconductive compound based on ethylene copolymer compound, designed for conductor screen and insulation shield applications in XLPE and EPDM insulated cables with bond.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ASTM D257 |
Trelleborg Horda Cable E7355-A4 Strippable Semiconductive Shielding E7355-A4 is a silane crosslinkable, strippable semiconductive compound for medium voltage cables.E7355-A4 meets the requirements as below, when optimal processing, extrusion and crosslinking procedu.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E7355-A4 Strippable Semiconductive Shielding E7355-A4 is a silane crosslinkable, strippable semiconductive compound for medium voltage cables.E7355-A4 meets the requirements as below, when optimal processing, extrusion and crosslinking procedu.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ASTM D257 |
Trelleborg Horda Cable E8406 Easy Strippable Semiconductive Shielding E8406 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8406 meets the requirements as be.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E8406 Easy Strippable Semiconductive Shielding E8406 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8406 meets the requirements as be.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E8409 Easy Strippable Semiconductive Shielding E8409 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8409 meets the requirements as be.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E8413 Easy Strippable Semiconductive Shielding E8413 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8413 meets the requirements as be.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ASTM D257 |
Trelleborg Horda Cable E8415 Easy Strippable Semiconductive Shielding E8415 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8415 meets the requirements as bel.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ASTM D257 |
Trelleborg Horda Cable E8502 Strippable Semiconductive Shielding E8502 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8502 meets the requirements as bel.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E8502 Strippable Semiconductive Shielding E8502 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8502 meets the requirements as bel.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E8551 Strippable Semiconductive Shielding E8551 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8551 meets the requirements as bel.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E8560 Strippable Semiconductive Shielding E8560 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8560 meets the requirements as bel.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ASTM D257 |
Trelleborg Horda Cable E8561 Strippable Semiconductive Shielding E8561 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8561 meets the requirements as bel.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E8561 Strippable Semiconductive Shielding E8561 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8561 meets the requirements as bel.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ASTM D257 |
Trelleborg Horda Cable E8900 Strippable Semiconductive Shielding E8900 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8900 meets the requirements as be.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E8900 Strippable Semiconductive Shielding E8900 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8900 meets the requirements as be.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ASTM D257 |
Trelleborg Horda Cable E7310 Bonded Insulation Shielding And Conductor Screen E7310 is a silane crosslinkable semiconductive compound for medium voltage cables. The material is designed as a conductor screen and bonded insulation shielding.E7310 meets the requirements as bel.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E7310 Bonded Insulation Shielding And Conductor Screen E7310 is a silane crosslinkable semiconductive compound for medium voltage cables. The material is designed as a conductor screen and bonded insulation shielding.E7310 meets the requirements as bel.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 120 °C |
<= 1000 ohm-cm @Temperature 248 °F |
ASTM D257 |
Trelleborg Horda Cable E8465 Easy Strippable Semiconductive Shielding E8551 is a vulcanizing, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8551 meets the requirements as bel.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
DC; ISO 3915 |
Borealis LE7704 Polyethylene Compound, Semiconductive, Thermoplastic LE7704 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7704 is intended for semiconductive applications in medium voltage.. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
DC; ISO 3915 |
Borealis LE7710 Polyethylene Compound, Semiconductive, Thermoplastic LE7710 is a thermoplastic black polyethylene compound, specially designed for semiconductive screen applications. Applications: LE7710 is intended for semiconductive applications in medium voltage .. |
|||
Volume Resistivity | <= 1000 ohm-cm @Temperature 90.0 °C |
<= 1000 ohm-cm @Temperature 194 °F |
ISO 3915 |
Borealis Supersmooth™ LE8280 Polyethylene Insulation Compound, Crosslinkable Supersmooth™ LE8280 is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Applications: Supersmooth™ LE8280 is intended for semiconduct.. |