Material Notes:
105°C; VW-1 rated non-lead stabilized insulation with good flexibility. Ideally suited for 1/64 wall (18 AWG and larger). UL approved for TW, THW, THHW applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.30 - 1.34 g/cc
1.30 - 1.34 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 94
88 - 94
delayed; ASTM D-2240
Tensile Strength, Yield 16.9 MPa
2450 psi
ASTM D-638
Elongation at Yield 264.3 %
264.3 %
Air Aging: 7 days @ 136°C; 30 mil slabs; UL 1581
283.5 %
283.5 %
Oil Aging: 96 hours @ 100°C; 30 mil slabs; UL 1581
330 %
330 %
ASTM D-638
100% Modulus 0.0124 GPa
1.80 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -24.0 °C
-11.2 °F
ASTM D-746
Oxygen Index 28 %
28 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+15 ohm-cm
1.50e+15 ohm-cm
50% RH; ASTM D-257
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F