Material Notes:
40 Shore hardness low viscosity injection mouldable liquid silicone rubber with high tear strength, high elongation and a fast cure speed.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc

@Temperature 25.0 °C
1.09 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 38
38
Tensile Strength, Ultimate 5.52 MPa
800 psi
Elongation at Break 500 %
500 %
Tear Strength 28.0 kN/m
160 pli
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+15 ohm-cm
1.50e+15 ohm-cm
Dielectric Constant 2.7

@Frequency 100 Hz
2.7

@Frequency 100 Hz
Dielectric Strength 30.3 kV/mm
770 kV/in
Dissipation Factor 0.00060

@Frequency 100 Hz
0.00060

@Frequency 100 Hz
Processing Properties Metric English Comments
Pot Life 4320 min
4320 min
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Appearance translucent
Hydrophobic yes
Mix Ratio (X:1) 100
Base to Catalyst ETN