Electrical Properties Metric English Comments
Dielectric Strength 6.00 kV/mm
152 kV/in
Pyrotek NT-C Electrical Insulating Material
NT-C offers superior arc and heat resistance properties, with adequate strength properties to withstand mechanical stress and hold up in severe electrical insulating applications. NT-C does not pro..
Dielectric Strength 6.00 kV/mm
152 kV/in
AC 60 Hz
Fujipoly Industries Sarcon® 20GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 6.00 kV/mm
152 kV/in
AC 60 Hz
Fujipoly Industries Sarcon® 20GSR Thin-Film GSR
Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of..
Dielectric Strength 6.00 kV/mm
152 kV/in
AC 60 Hz
Fujipoly Industries Sarcon® 20GSR Thin-Film GSR
Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of..
Dielectric Strength 6.00 kV/mm
152 kV/in
150°C for 1,000 hrs
Fujipoly Industries Sarcon® 20GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 6.00 kV/mm
152 kV/in
60°C for 500 hrs
Fujipoly Industries Sarcon® 30GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 6.00 kV/mm
152 kV/in
60°C for 500 hrs
Fujipoly Industries Sarcon® 30T Thin-Film TR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 6.00 kV/mm
152 kV/in
200°C for 1,000 hrs
Fujipoly Industries Sarcon® 45H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 6.00 kV/mm
152 kV/in
60°C for 500 hrs
Fujipoly Industries Sarcon® 85H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 6.00 kV/mm
152 kV/in
Step by Step; ASTM D149
Plenco 00732 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007..
Dielectric Strength 6.00 kV/mm
152 kV/in
AC Rapid Rise; ASTM D149
DuPont™ Nomex® N196 Paper, 10 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Dielectric Strength 6.00 kV/mm
152 kV/in
AC Rapid Rise; ASTM D149
DuPont™ Nomex® N196 Paper, 15 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Dielectric Strength 6.00 kV/mm
152 kV/in
AC Rapid Rise; ASTM D149
DuPont™ Nomex® N196 Paper, 20 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Dielectric Strength 6.00 kV/mm
152 kV/in
AC Rapid Rise; ASTM D149
DuPont™ Nomex® N196 Paper, 7 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Dielectric Strength 6.00 - 8.00 kV/mm

@Temperature 90.0 °C
152 - 203 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit..
Dielectric Strength 6.00 - 8.00 kV/mm

@Temperature 90.0 °C
152 - 203 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATO 145 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium flow Applications: Electric ..
Dielectric Strength 6.00 kV/mm
152 kV/in
dry; IEC 60243-1
EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF
Information provided by EMS Grivory
Dielectric Strength 6.00 kV/mm
152 kV/in
conditioned; IEC 60243-1
EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF
Information provided by EMS Grivory
Dielectric Strength 6.00 - 35.0 kV/mm
152 - 889 kV/in
Average value: 20.3 kV/mm Grade Count:3
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..