Plenco 00732 Melamine-Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Melamine , Melamine-Phenolic Copolymer , Phenolic
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 00732 Melamine-Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00732 is available in a wide range of colors.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.660 g/cc
0.0238 lb/in³
ASTM D1895
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Water Absorption 0.46 %
0.46 %
ASTM D570
Linear Mold Shrinkage 0.0093 cm/cm
0.0093 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 85
85
ASTM D785
Tensile Strength, Ultimate 65.0 MPa
9430 psi
ASTM D638
Elongation at Break 0.89 %
0.89 %
ASTM D638
Tensile Modulus 9.00 GPa
1310 ksi
ASTM D638
Flexural Strength 97.0 MPa
14100 psi
ASTM D790
Flexural Modulus 8.10 GPa
1170 ksi
ASTM D790
Compressive Strength 194 MPa
28100 psi
ASTM D695
Poissons Ratio 0.36
0.36
ASTM D638
Shear Modulus 3.31 GPa
480 ksi
Calculated
Izod Impact, Notched 0.168 J/cm
0.315 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.216 J/cm²
1.03 ft-lb/in²
ASTM D256
Impact 106
106
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature 40.0 - 130 °C
29.4 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 140 °C
284 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 186 °C
367 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.610 mm
V-0

@Thickness 0.0240 in
Oxygen Index 33 %
33 %
ASTM D2863
Shrinkage 1.24 %
1.24 %
240 hr, 105ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 9.70e+12 ohm-cm
9.70e+12 ohm-cm
ASTM D247
Dielectric Constant 7.7
7.7
ASTM D150
Dielectric Strength 6.00 kV/mm
152 kV/in
Step by Step; ASTM D149
9.20 kV/mm
234 kV/in
Short Time; ASTM D149
Dissipation Factor 0.064
0.064
ASTM D150
Arc Resistance 185 sec
185 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638