Plenco 4224 Phenolic, Granular, Transfer Molded  (discontinued **)

Category Polymer , Thermoset , Phenolic , Phenolic; Unreinforced; Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4224 Phenolic, Granular, Transfer Molded  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-stage Phenolic. PLENCO 04224 is a brown, two stage, general purpose phenolic molding compound. It has good electrical and moldability characteristics. It is used in electrical and automotive applications and can be molded by compression, transfer, or injection processes.Information supplied by Plenco
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Apparent Bulk Density 0.600 g/cc
0.0217 lb/in³
Apparent density per ASTM D1895
Water Absorption 0.35 %
0.35 %
ASTM D570
Linear Mold Shrinkage 0.0062 cm/cm
0.0062 in/in
per ATM D955. Post shrinkage is 0.23% at 72hr 120ºC per ASTM D1299.
Mechanical Properties Metric English Comments
Hardness, Rockwell E 91
91
ASTM D785
Tensile Strength, Ultimate 54.3 MPa
7880 psi
ASTM D638
Elongation at Break 0.72 %
0.72 %
ASTM D638
Tensile Modulus 8.64 GPa
1250 ksi
ASTM D638
Flexural Yield Strength 84.1 MPa
12200 psi
ASTM D790
Flexural Modulus 8.00 GPa
1160 ksi
ASTM D790
Compressive Yield Strength 218.9 MPa
31750 psi
ASTM D695
Izod Impact, Notched 0.210 J/cm
0.393 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ASTM D256
Impact 120
120
J/m Plenco drop ball test
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 195 °C
383 °F
Heat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 185 °C
365 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.10 mm
V-0

@Thickness 0.240 in
Electrical Properties Metric English Comments
Electrical Resistivity 3.42e+11 ohm-cm
3.42e+11 ohm-cm
ASTM D257
Dielectric Constant 5.0

@Frequency 1e+6 Hz
5.0

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 12.2 kV/mm
310 kV/in
Short Time; ASTM D149
Dissipation Factor 0.051

@Frequency 1e+6 Hz
0.051

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 120 sec
120 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638